kaperomako
kaperomako
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 199
kind attention. i am trying to cover the fenders of my car in CF. but i got some trouble with the materials that i have to use. i live in the dominican republic, and i can not purchase from easy composites big parts of the materials needed as black epoxy base coat and laminating resin.
i would like to know if there are any substitute that could be use for this job. ex. i found on ebay the black epoxy for the first layer but in small qunatity and it doesn't get the job done. could i skin the whole part just using normal epoxy resin or could some one give me an idea.
thanks.
Reply
Like
2
ajb100
ajb100
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
I use normal resin mixed with graphite powder as a black base coat
Reply
Like
2
ebf2k
ebf2k
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 9,
Visits: 28
As long as what you are skinning is black then you can use your laminating resin for the base coat. The base coat is black so if there are any gaps in the fabric you don't see the other color underneath.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search