1. We don't have a specific graph from the manufacturer, only the basic specification of 10% shrinkage at 80C.
2. Release coating is on one side, the side facing the inner carboard roll.
3, 4, 5. not presently

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
michael.sellers@oxinst.com...
michael.sellers@oxinst.com
Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)
Group: Forum Members
Posts: 1, Visits: 3
Can I get a technical data sheet for your high shrink tape? The questions I need to answer:

  1. What does the shrinkage force vs temperature graph look like?
  2. Is its release coating on both sides or only one? If only one, which one?
  3. Do you offer any alternative thicknesses?
  4. Do you offer any different types, e.g. with different shrink %age vs temperature?
  5. Do you offer any different finishes? e.g. perforated to help out-gassing?
Regards, Mike.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search