Can I get a technical data sheet for your high shrink tape? The questions I need to answer:

  1. What does the shrinkage force vs temperature graph look like?
  2. Is its release coating on both sides or only one? If only one, which one?
  3. Do you offer any alternative thicknesses?
  4. Do you offer any different types, e.g. with different shrink %age vs temperature?
  5. Do you offer any different finishes? e.g. perforated to help out-gassing?
Regards, Mike.
By Warren (Staff) - 9/9/2013 11:13:25 AM

Answers:

1. We don't have a specific graph from the manufacturer, only the basic specification of 10% shrinkage at 80C.
2. Release coating is on one side, the side facing the inner carboard roll.
3, 4, 5. not presently