Brake Ducts
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Dom_962
Dom_962
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 9
Hey guys
I'm wanting to make some
resin infused carbon fibre brake ducts.. these will be the backing plate as well.. these will have a airflow from the the front bumper flowing through them at most times..
I'm wanting to know if standard (3k) carbon fibre sheet can be use with the standard infusion process or will i need something else or do i need to do a wet lay up style.. the current backing plates are made out of tin..??
Any advice would be greatly appreciated..
Cheers
Dominic Martens
Tags
Brakes
resin infusion
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Brake Ducts
Dom_962
-
13 Years Ago
Standard woven fabrics will be fine for making the duct and can be used with infusion no problem.
Warren (Staff)
-
13 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search