Group: Forum Members
Posts: 18,
Visits: 52
|
GC50 is a good product, It's one of the few Polyester gelcoats that works very well with Epoxy underlays and adheres well.
Yes, paint or spray GC50 into the mould, allow to cure for the recommended inteval and then laminate onto it.
|