	Group: Administrators 	        
    Posts: 2.5K, 
    Visits: 8.5K 
    
 
          
		     | 
				                       
                 
                
                    
			            If you can, embed them now, preferably with a load spreading washer or similar screwed on.  Carbon doesnt like raw threads so much so you can easily rip out a screw or similar if its not bonded in properly or doesnt have any way of spreading the load over an area.                
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |