Since there has been no reply I'll post results of the products I used. When they arrive...

I'm using Mazerna (sp?) polishing compounds and they do the trick nicely, in combination  wet and dry up to about 1200 grit.
Edited 12 Years Ago by LaxFriedrichs
LaxFriedrichs
LaxFriedrichs
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 58, Visits: 450
There are small regions on my mould that are hard to get to with wet & dry paper. Could anyone recommend suitable abrasive compound to use in conjunction with my dremel tool and a felt bit?

Cheers,
Adam
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search