There are small regions on my mould that are hard to get to with wet & dry paper. Could anyone recommend suitable abrasive compound to use in conjunction with my dremel tool and a felt bit?
Cheers,
Adam
By LaxFriedrichs
-
8/13/2013 2:59:00 PM
Since there has been no reply I'll post results of the products I used. When they arrive...
I'm using Mazerna (sp?) polishing compounds and they do the trick nicely, in combination wet and dry up to about 1200 grit.