	Group: Awaiting Activation 	        
    Posts: 6, 
    Visits: 40 
    
 
          
		     | 
				                       
                 
                
                    
			            Hi. I would like to use your 12mm protruded tube for a multicopter motor arm but would like to end up with a square end to hinge the arm. Looking at your sizes it would seem the best way to achieve this is :- 12mm (OD) protruded tube inside 12.5mm (ID) wrapped tube inside 20mm carbon box.
  I already have your 12mm protruded tube and it measures 12.3mm which may be a problem if the the 12.5mm ID wrapped tube is smaller than advertised.
  Could you please check the fit before I order. They will be glued together with epoxy.
  Thanks
  Vince                
			            				
			                                 
                     
                                            
                         
                    
                  
             |