By Vince - 8/5/2013 12:13:31 PM
Hi. I would like to use your 12mm protruded tube for a multicopter motor arm but would like to end up with a square end to hinge the arm. Looking at your sizes it would seem the best way to achieve this is :- 12mm (OD) protruded tube inside 12.5mm (ID) wrapped tube inside 20mm carbon box.
I already have your 12mm protruded tube and it measures 12.3mm which may be a problem if the the 12.5mm ID wrapped tube is smaller than advertised.
Could you please check the fit before I order. They will be glued together with epoxy.
Thanks
Vince
|
By Vince - 8/5/2013 6:17:09 PM
Excellent. Thanks.
|
|