Hi Daz.
Getting the glass was pretty straight forward I looked around local glass suppliers until I found the best deal (£250 negotiated), the one you see for the table cover is standard size 2.44m x 1.22 m x 6mm toughened glass so there was no need for any modifications to fit on a standard 19mm multiply ply-board and I was lucky to get the holes drilled for free so just ask your local company for a great deal and tell them it is for a project.
A much cheaper option is to use perspex sheet and the best deal around is from a company called MP Plastic Building Products Ltd www.plasticproductsuk.co.uk .I am going to get a top-sheet of 6mm clear perspex sheet for my table which is so much more lighter to handle on and off the table to make perfect laminate plates, and from this company and I was quoted £167.59 which includes VAT and P&P delivered to the workshop which is another bargin.
Good luck with your search and hoping you can get a good deal too.
Jim
|