Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Clear bar tops
Clear bar tops
Post Reply
Like
2
Clear bar tops
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Snoozer
Snoozer
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 8
I am a bar fitter and have been asked to install a wooden bar top cove with coins and then covered with resin. This is quite popular in the US and there are lots of products available, however the In the UK I can't find andy reference to suitable epoxy resins.
They tend to be self levelling, clear and bubbles worked out with a heat gun...
Ta
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Clear bar tops
Snoozer
-
12 Years Ago
The best way to do it withresins is with our Waterclear Polyurethane Casting Resin . You will...
Warren (Staff)
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search