I am a bar fitter and have been asked to install a wooden bar top cove with coins and then covered with resin.  This is quite popular in the US and there are lots of products available, however the In the UK I can't find andy reference to suitable epoxy resins.

They tend to be self levelling, clear and bubbles worked out with a heat gun...

Ta
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K

The best way to do it withresins is with our Waterclear Polyurethane Casting Resin.  You will need to do the pouring in a dry andwarm room preferably over 25C and pour at least a minimum of 2mm thick over thetop level of any coins, preferably a bit thicker.

 

You will need to put some kind of dust shieldover the top to ensure no dust or bugs land in the resin while it cures.

 

The far cheaper way I suspect would be a sheet oftoughened glass over the top, although that may not be what the client wants.



Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search