I'm planning to make motorcycle trousers out of kevlar fabric but am not sure what I should choose. The plan is to make a pair of trousers out of kevlar, rather than making them from normal fabric and reinforcing the knees, hips and bum. There is so much choice here and I am spoiled for choice! Can anyone let me know which fabric would be best for making a garment?
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You are best looking at the fabrics within our KevlarProtective Textiles range of products.

You would be looking at a multi layer garment as raw kevlar would unlikely give you the external finish wanted in most motorbike clothes. 

Depending on your design you could be using a combination of the textile materials above in different places of the garment.

Be aware that motorbike clothing manufacturers often put thier garments through extensive R&D and testing to get the desired performance so you need to be careful to ensure you have adequate protection and arent making a garment that may fail causing you more injurys than otherwise with a tested bit of kit.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search