Group: Forum Members
Posts: 12,
Visits: 32
|
You ideally want to apply the vacuum as quickly as possible upon finishing the laminate and making sure the consumables are placed and setup correctly. It the resin starts to gel then you run the risk of the laminate not being consolidated properly.
|