I have constructed a carbon fiber tube, which I will glue an anodized aluminum sleeve on each end ..
There will be tension and compression in the aluminum sleeves.
Which glue you recommend?
Thanks for your help.
Magnus


 

Paul (Staff)
Paul (Staff)
Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi Magnus,

The best adhesive for composite to metal would be an epoxy based one, in your case with close fitting inserts I would advise using the ET515 15minute system, this has proven itself to offer very reliable and strong bonds in these conditions.

Paul Statham
Easy Composites / Carbon Mods - Technical
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search