By batbyggare - 2/13/2012 8:34:05 PM
I have constructed a carbon fiber tube, which I will glue an anodized aluminum sleeve on each end .. There will be tension and compression in the aluminum sleeves. Which glue you recommend? Thanks for your help. Magnus
|
By Paul (Staff) - 2/14/2012 9:25:44 AM
Hi Magnus,
The best adhesive for composite to metal would be an epoxy based one, in your case with close fitting inserts I would advise using the ET515 15minute system, this has proven itself to offer very reliable and strong bonds in these conditions.
|
|