ok so i set about making my first mould. as some of you know ive had to use polyester resin as i was misinformed before i purchased my supplies. anyway ive got a few questions to go with the pics ive uploaded. why did the pva bead off? i assume its not compatible with the wax. i cleaned it from the part and just waxed it again as i didnt want these beads in the mould.

can i use the tooling gelcoat again with carbon fibre or chopped strand to reinforce the mould? or can i use epoxy laminating resin over the cured polyester to reinforce it?

thanks


Attachments
IMG-20120211-00038.jpg (262 views, 428.00 KB)
IMG-20120211-00039.jpg (231 views, 400.00 KB)
IMG-20120211-00040.jpg (243 views, 450.00 KB)
IMG-20120211-00041.jpg (236 views, 249.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search