Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
first mould
first mould
Post Reply
Like
3
first mould
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
japcarmaniac
japcarmaniac
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 53,
Visits: 157
ok so i set about making my first mould. as some of you know ive had to use polyester resin as i was misinformed before i purchased my supplies. anyway ive got a few questions to go with the pics ive uploaded. why did the pva bead off? i assume its not compatible with the wax. i cleaned it from the part and just waxed it again as i didnt want these beads in the mould.
can i use the tooling gelcoat again with carbon fibre or chopped strand to reinforce the mould? or can i use epoxy laminating resin over the cured polyester to reinforce it?
thanks
Attachments
IMG-20120211-00038.jpg
(
261 views,
428.00 KB
)
IMG-20120211-00039.jpg
(
230 views,
400.00 KB
)
IMG-20120211-00040.jpg
(
242 views,
450.00 KB
)
IMG-20120211-00041.jpg
(
235 views,
249.00 KB
)
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
first mould
japcarmaniac
-
13 Years Ago
update! the mould turned out good today. i noticed that were i had left the pva on the board there...
japcarmaniac
-
13 Years Ago
Nice to hear that it turned out good. I never ever used PVA and never had bad news. BUT on a plug...
Joe
-
13 Years Ago
nice to hava another belgian compagnon here ;) OT: I mostly wax and polish my mould 4times then...
matthieutje65
-
13 Years Ago
yeh i noticed that. ive givin the mould about 7 waxes already and smoothed down a little lip that...
japcarmaniac
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search