Hello all,

I need to make a two part mould of an object made of wood that's surface is lacquered, but I'm very keen not to damage the object.

Could you recommend the best suited molding method for this? The piece no larger that 600mm x 400mm x 150mm. The mold should be reusable also.

Many thanks,
Adam
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
LaxFriedrichs - 12 Years Ago
carboncactus - 12 Years Ago
LaxFriedrichs - 12 Years Ago
matthieutje65 - 12 Years Ago
LaxFriedrichs - 12 Years Ago
carboncactus - 12 Years Ago
LaxFriedrichs - 12 Years Ago
carboncactus - 12 Years Ago
LaxFriedrichs - 12 Years Ago
                                     Is your mould going to be subject to heat? i.e. postcured, used for prepreg? If not, you might have...
carboncactus - 12 Years Ago
                                         There will be no heat in the process. I will be doing resin infusion. Will tell you how I get...
LaxFriedrichs - 12 Years Ago
                                         One extra remark, make sure your wood is sealed, the exotherm reaction, creating heat, could make...