Group: Forum Members
Posts: 93,
Visits: 651
|
the wings weigh 3lb
the front valance weighs 5 lb but that was without trimming it out of the mold
The original wings were just under 10 lb
The front valance was 13lb
The doors & bonnett ,boot are the real weight savers