By Daz - 5/31/2013 11:17:32 PM
This is what ive done in the past few months for my car
I have also done a roof , 4 doors and a lot of other bits LOL, Made a dashboard,
 Made it so it goes around the roll cage and door bars 3lb in weight the original is 13lb
 Also started the rear air intakes for the rear rad conversion





 Also made one of the air scoops

 Also made the air box for the rad I have made it small as i want to keep the air pressure up inside Its divided as well Some of the air boxs ive seen open up too much causing a pressure drop.

 Also made a box for my pro alloy fuel tank as it sits behind me
 Also made one of the front wings at last 3 piece mold and it worked fine
 bit of fettling req but all good fitted one of the arches up ive made

 3.5 lb in weight compared to 15lb
Having never done any fiberglasing or carbon work before this
Im really happy with the outcome and ease of use of the easycomp system :-)
|
By Daz - 6/9/2013 8:53:06 PM
front end trial fitted to car ,
A little bit of fettling req but not too bad

Now with carbon Kevlar bonnet
|
|