This is what ive done in the past few months for my car
I have also done a roof , 4 doors and a lot of other bits LOL,
Made a dashboard,

Made it so it goes around the roll cage and door bars
3lb in weight the original is 13lb

Also started the rear air intakes for the rear rad conversion






Also made one of the air scoops


Also made the air box for the rad
I have made it small as i want to keep the air pressure up inside
Its divided as well
Some of the air boxs ive seen open up too much causing a pressure drop.


Also made a box for my pro alloy fuel tank as it sits behind me

Also made one of the front wings at last
3 piece mold and it worked fine

bit of fettling req but all good
fitted one of the arches up ive made


3.5 lb in weight compared to 15lb
Having never done any fiberglasing or carbon work before this
Im really happy with the outcome and ease of use of the easycomp system :-)