The best way is with either a metal insert that slides closely into the inside of the tube, or a sleeve on the outside.

That way you can then bond over a large surface area which means the loads are spread over a greater area which is ideal way to get a nice strong bond.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
hietaka
hietaka
Supreme Being (172 reputation)Supreme Being (172 reputation)Supreme Being (172 reputation)Supreme Being (172 reputation)Supreme Being (172 reputation)Supreme Being (172 reputation)Supreme Being (172 reputation)Supreme Being (172 reputation)Supreme Being (172 reputation)
Group: Forum Members
Posts: 14, Visits: 169
Hi.

is it any idea to connect and bond a carbon tube to a metal joint  strongly?

I want to build a vehicle that is something like bike.
to build the vehicle, I will use some carbon tubes and metal joints.
and I will bond the tube and the joint.

but I don`t know the best way to bond them.

Is it enough strong if I insert the tube into the joint and bond them?
because of shocks and vibration, the connection will be broken in the future?

or should I reinforce the connection after I bond the tube and the joint?and how to do that?

Thanks,

Hietaka
Japan


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search