How to have a clean break lines between joints.
How to have a clean break lines between joints.
Post Reply
Like
1
How to have a clean break lines between joints.
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
SIL1580
SIL1580
posted 12 Years Ago
ANSWER
Topic Details
Group: Forum Members
Posts: 4,
Visits: 94
Hi... im not sure this topic is up before. I would like to ask... How to have a clean and strait joint lines in between 2 carbon sheets? Lets say using the carbon skinning technics.
THANKS IN ADVANCE!
Edited
12 Years Ago by
SIL1580
Reply
Like
1
carboncactus
carboncactus
posted 12 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
With prepreg, I make sure I have one piece that has a clean cut, preferably along the warp or weft. Then I just lay another over the top, overlapping the join. I think you should be able to do the same if you wanted to skin. I would tackify the cloth with some cheap hairspray (cheapest possible, don't want any perfumes). You'll essentially have a cloth that behaves like prepreg but without the resin if that makes sense. You can then cut it cleanly and lay it on the part.
Reply
Like
1
SIL1580
SIL1580
posted 12 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 4,
Visits: 94
Thank you so much carboncactus... u really light up my day. I absolutely got what u mean... very useful trick. Thanks!
Reply
Like
1
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
1
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search