Group: Forum Members
Posts: 61,
Visits: 558
|
I've seen it mentioned before on here - but wasn't available in less than 25kg - quite popular in marine use I understand - I guess the issue is still whether a brushed coat of clear is uniform enough to not distort the weave underneath - obviously when pigmented there's no issue... If so then you are still back to needing to spray the gel...