By GROPIUS - 5/7/2013 8:51:07 PM

Hi again,
I've been looking for an alternative to the GC50 when applied by brush.
As the GC50 has been proven to be a right pick and frustrating to work with...
By jamesw - 5/8/2013 12:19:36 PM

I've seen it mentioned before on here - but wasn't available in less than 25kg - quite popular in marine use I understand - I guess the issue is still whether a brushed coat of clear is uniform enough to not distort the weave underneath - obviously when pigmented there's no issue... If so then you are still back to needing to spray the gel...