kind attention.  need some help about "cleaning" out the residues let by the 3m composite spray glue. although my part is not 100% finish, i will like to try the process that matthieutje65 use for his carbon fiber helmet. but i was wondering if this residue will be annoying and get my part ugly.

can anyone help me with what to use in order to clean up my part.
Attachments
IMG-20130422-01738.jpg (206 views, 256.00 KB)
IMG-20130422-01740.jpg (180 views, 406.00 KB)
IMG-20130422-01742.jpg (172 views, 394.00 KB)
IMG-20130422-01741.jpg (162 views, 432.00 KB)
IMG-20130422-WA006.jpg (177 views, 81.00 KB)
IMG-20130422-WA005.jpg (183 views, 112.00 KB)
Replies
kaperomako
kaperomako
Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)Junior Member (22 reputation)
Group: Forum Members
Posts: 4, Visits: 199
well matthieutj65, you have been  very helpful.  keep posting my advance in the project.

well although the final part did not when 100% like a pro. for my 1st time, i think it when very well. the process takes time but the results and the knowledge acquire was very exciting.  the last part of the engine cover is the holes that attach it to the engine. i am thinking of pasting some insert or any advice??
Attachments
IMG-20130430-01802.jpg (177 views, 398.00 KB)
IMG-20130430-01801.jpg (208 views, 478.00 KB)
IMG-20130430-01798.jpg (168 views, 317.00 KB)
IMG-20130430-01796.jpg (185 views, 423.00 KB)
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
you're welcome! looks like a job well done!

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search