Nearly got a set to mould off for my bike but think I will build them straight off the frame. 
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Below is an image of one of a pair of frame guards i am making for a Kawasaki 750 race bike ( pre trimmed ), when i made the moulds i made the flanges quite narrow as i was going to use wet lay but i have used infusion for this part. The flange is just wide enough if i am careful fitting the mesh and infusion connectors. I have used EC products throughout . 



http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Edited 12 Years Ago by Bartonphoenix750
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search