Hi

would it work to infuse a carbon braided sleeve?
Multiple layers?
Inside a tube mould, the 80mm sleeve.
To be more specific, would the resin flow good in a sleeve?
I have quite good understanding for the method of bagging etc.
(enveloped bag folded bag over itself and the mold.)

(by the way, isn't something wrong in the product description of the 80mm?)


/Petter


http://motoform.blogspot.se

Edited 13 Years Ago by prsw
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
prsw - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search