By prsw - 4/18/2013 8:12:33 PM				
            
                      
            Hi
  would it work to infuse a carbon braided sleeve? Multiple layers? Inside a tube mould, the 80mm sleeve. To be more specific, would the resin flow good in a sleeve? I have quite good understanding for the method of bagging etc. (enveloped bag folded bag over itself and the mold.)
  (by the way, isn't something wrong in the product description of the 80mm?)
 