Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pattern and Plug Making
»
Caterham/Lotus 7 Cycle Wing
Caterham/Lotus 7 Cycle Wing
Post Reply
Like
3
Caterham/Lotus 7 Cycle Wing
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Another weekend of woodwork, shaping, filling, sanding and spraying. This time its a plug for a front Cycle Wing for a Caterham 7 race car.
Regards Warren
Carbon
Copies Ltd
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Caterham/Lotus 7 Cycle Wing
wozza
-
12 Years Ago
Looks good. Any idea on the required layup? I have some carbon cycle wings on my Seven, but they...
Mavenl
-
12 Years Ago
Got the mould done and the first test piece infused in GRP. Hi Marcel, the planned layup is 200grm...
wozza
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search