Another weekend of woodwork, shaping, filling, sanding and spraying. This time its a plug for a front Cycle Wing for a Caterham 7 race car.
Regards Warren
By wozza
-
4/17/2013 10:24:28 PM
Got the mould done and the first test piece infused in GRP.
Hi Marcel, the planned layup is 200grm - 200grm - 2mm Soric - 200grm