Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Peel Ply
Peel Ply
Post Reply
Like
3
Peel Ply
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
expunged
expunged
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 3
After doing the vacuum bag and peeling the peel ply in your bonnet video, the surface that the peel ply was on seems dull, can this be buffed to a shine or will it remain dull?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Peel Ply
expunged
-
12 Years Ago
it could be wet sanded and polished if needed or wet sanded and clearcoated
neilb
-
12 Years Ago
Its supposed to have a coarse texture, to act as an ideal bonding surface without prior preparation....
baja_patient
-
12 Years Ago
An alternative if you want a great finish is when you make the inner mould, mould the underside of...
Warren (Staff)
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search