THX Warren

I used it yesterday laying up the final layers on the molds, worked ok but a bit unusual to remove the air under the CSM.

Ok, I did a compression molded laminate with 1,4 coremat with 2 layers of 200g 2x2 on each side and got a very strong and light sandwich,
buy I will follow your advise and go for foam, I have lots of bonocell and diviny cell.


Warren (Staff) (05/04/2013)
Coremat will be fine upto a max of 100C when used in mould making to add thickness while saving using fibreglass.

I certainly would NOT recommend coremat in ANY carbon part as it is a very low performance core that soaks up a lot of resin.  Better core materials are not that much more expensive and include Closed Cell Foam Core and  2mm Lantor Soric.



http://motoform.blogspot.se

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Coremat will be fine upto a max of 100C when used in mould making to add thickness while saving using fibreglass.

I certainly would NOT recommend coremat in ANY carbon part as it is a very low performance core that soaks up a lot of resin.  Better core materials are not that much more expensive and include Closed Cell Foam Core and  2mm Lantor Soric.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
prsw
prsw
Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)
Group: Forum Members
Posts: 112, Visits: 1K
Would Lantor coremat be suitable as reinforcement in a mold made with unimold?
The mold will be heat treated and when used for molding the parts will be cured under heat, in mold.

also, would Lantor coremat be suitable as sandwich material in a carbon part made for a high temp application?


http://motoform.blogspot.se

Edited 13 Years Ago by prsw
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search