Group: Forum Members
Posts: 1,
Visits: 15
|
We have successfully infused components on our race car. A few mistakes but its a great clean way to make parts.
We have used expanded green foam to add modulus in different areas to add stiffness in parts. Works great and does not soak up any epoxy.
But can we use lighter polystyrene white foam and not have the epoxy soak into the foam?
Any suggestions?
Thank you
J Beninca
|