Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Material Properties for Chopped strand mat fibreglass
Material Properties for Chopped strand mat fibreglass
Post Reply
Like
24
Material Properties for Chopped strand mat fibreglass
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Richard
Richard
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 4
do you have data for the material properties of the various chopped strand mats on the site after being combined with polyester resin, data for combining with epoxy resin would also be appreciated
in particular
density
tensile modulus
compressive modulus
(failing these a general youngs modulus)
ultimate tensile strength
ultimate compressive strength
poissons ratio
any help would be greatly appreciated
Tags
compressive
material propeties
modulus
tensile
Reply
Like
24
Warren (Staff)
Warren (Staff)
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
CSM is rarely used as a "High performance" laminate so as a result we have struggled to find the data you want online. I imagine it probably exists in paper format and just hasnt migrated onto online as most of the traditional users of CSM will already be aware of the material properties.
We have been able to find some representative data for 450gsm CSM in a Polyester resin based laminate with 31% of the matrix being glass.
PROPERTY METHOD UNIT RESUL
T
Tensile Strength IS03268/DIN53455 Mpa 108
Tensile Elongation IS03268/DIN53455 % 1.8
Tensile Modulus IS03268/DIN53455 Mpa 7800
Flexural Modulus ISO 178 Mpa 6770
Flexural Strength ISO 178 Mpa 204
Flexural Elongation ISO 178 % 3.4
The only way to get more data would be a
pproaching
the manufacturer directly of the specific
chopped strand matt that you want to use and seeing if they
hold a electronic file they can send or scan a paper copy.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Edited
13 Years Ago by
Warren (Staff)
Reply
Like
16
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
24
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search