Dear Sir/Madam

I`d like order material for repair carbon frame ( see the attached file) but I never use carbon.

I will use this for the first time so I`d like to ask you what I will be need for this repair.

Can you give me some advice about how I can do this repair and how I can use this material?

My last question is that can you tell me how much cost postage to the Slovakia?

I look forward to hearing from you.

Have a nice day. 

Regards,

Peter Adámek


Attachments
DSC_0004.JPG (241 views, 170.00 KB)
DSC_0005.JPG (217 views, 101.00 KB)
DSC_0006.JPG (212 views, 87.00 KB)
DSC_0008.JPG (216 views, 85.00 KB)
DSC_0009.JPG (210 views, 81.00 KB)
DSC_0010.JPG (205 views, 94.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search