Hi , whats the epoxy amount for

300g diolen                                        

3mm Soric    

all so i have the breather cloth in my infussion kit,but its not mensioned in the video?  do i use it ?

i have a male corner in my mould and have cut the material to fold around it, is it possible to tack down the skicky out bits within the mould, if so what with? 

i am using wax ontop off a pva (polyester resin mould) as a release will this be ok

 

many thanks  


Edited 14 Years Ago by jackflash
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search