Hi , whats the epoxy amount for

300g diolen                                        

3mm Soric    

all so i have the breather cloth in my infussion kit,but its not mensioned in the video?  do i use it ?

i have a male corner in my mould and have cut the material to fold around it, is it possible to tack down the skicky out bits within the mould, if so what with? 

i am using wax ontop off a pva (polyester resin mould) as a release will this be ok

 

many thanks  


Edited 14 Years Ago by jackflash
Reply
Joe
Joe
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Also i just noticed you are using polyester mold with your epoxy part. Then you need to pay extra attention to surface preparation. The first part i ever made was a carbon/epoxy part made in a polyester mold. Thats not the better idea ever, however, waxing my mold 12 times (maybe a bit overdone héhé) lead to decent release properties. I had to use a little of pressurised air persuasion, but mold had many tight curves. Also, I heared that polyester mold would shrink a bit with time going by.

As most people here would say, always use compatible products to work with. Epoxy mold for epoxy parts, polyester molds for polyester parts. You can also find "multi purpose" products, that will work with epoxy, polyester and vinylester. On EC website, they have this.

Cheers from Belgium.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search