In terms of resins, our High Temperature Epoxy Laminating Resinwill go upto 180C. You would need to postcure the mould upto the planned operating temperature.

In terms of mould thickness, it depends on the moulds you are copying. If you are copying them exactly then you could probably reduce the thickness a little bit to take into account the extra stiffness that a carbon laminate will have compared to basic glass fibres.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
may I ask you why you would like to replace the Fiberglass moulds into CF-Moulds?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Brad 612
Brad 612
Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)
Group: Forum Members
Posts: 2, Visits: 14
Hi I am looking for info on methods to make carbon fibre moulds to be used in the plastic rotational moulding process,we have fibre glass mouldings 
With flanges that would directly make the finished moulds in cf,the questions are what would be the best resin to use at high  temperature  and what would be a good finished mould thickness to allow for long life and fast heating in the process oven, any advice will be appreciated brad 

Tags: 
Rotational moulding 

Edited: Yesterday @ 23:25:08 by Brad 612
Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search