TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
i got this video interesting only not understood what he lay before carbon cloth? any ideas? i thought only release agent good but he lay with brush something?
http://www.youtube.com/watch?v=8C0DkROWsiE
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
interesting carbon seats manufacture
TomDesign
-
12 Years Ago
first release-agent, then some kind of transparent gelcoat (topcoat), then spray and CF.
matthieutje65
-
12 Years Ago
That's a tacky spray. It's used to "hold" the fabric in place. Something like a glue in spray. IT...
nmicro
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search