By TomDesign - 2/26/2013 12:00:58 PM

i got this video interesting only not understood what he lay before carbon cloth? any ideas? i thought only release agent good but he lay with brush something?

http://www.youtube.com/watch?v=8C0DkROWsiE
By nmicro - 2/28/2013 12:09:00 AM

That's a tacky spray.  It's used to "hold" the fabric in place. Something like a glue in spray. 