Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
basic vac setup
basic vac setup
Post Reply
Like
2
basic vac setup
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
brasco
brasco
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 192,
Visits: 305
found this too.
Basic Vacuum Bagging Set-Up
by
daldrich@fibreglast.com
Vacuum Bagging
is a technique employed to create mechanical pressure on a laminate during its cure cycle. Pressurizing a composite lamination serves several functions. First, it removes trapped air between layers. Second, it compacts the fiber layers for efficient force transmission among fiber bundles and prevents shifting of fiber orientation during cure. Third, it reduces humidity. Finally, and most important, the vacuum bagging technique optimizes the fiber-to-resin ratio in the composite part.
The following diagram shows a basic vacuum bagging set-up:
CarbonFiberCreations
Reply
Like
2
brasco
brasco
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 192,
Visits: 305
feel free to add any knowledge to this thread.
thanks
scott
this is a basic vac setup from a web page where a guitar neck was being made.
CarbonFiberCreations
Attachments
Vac-Bag.png
(
252 views,
18.00 KB
)
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search