2/25/2013 1:20:29 AM
feel free to add any knowledge to this thread.
thanks
scott
this is a basic vac setup from a web page where a guitar neck was being made.
By brasco
-
2/25/2013 1:22:24 AM
found this too.
Basic Vacuum Bagging Set-Up
by
daldrich@fibreglast.com
Vacuum Bagging
is a technique employed to create mechanical pressure on a laminate during its cure cycle. Pressurizing a composite lamination serves several functions. First, it removes trapped air between layers. Second, it compacts the fiber layers for efficient force transmission among fiber bundles and prevents shifting of fiber orientation during cure. Third, it reduces humidity. Finally, and most important, the vacuum bagging technique optimizes the fiber-to-resin ratio in the composite part.
The following diagram shows a basic vacuum bagging set-up: