	Group: Administrators 	        
    Posts: 2.5K, 
    Visits: 8.5K 
    
 
          
		     | 
				                       
                 
                
                    
			            Table shows typical empiracle values for Easy Composites' carbon fibre pultruded tubes, strips and box sections. The testing was carried out to standards under ASTM D638/GB1447-83 as a representative test for the performance of the fibres rather than an exact measurement for each of the different box sections/pultrusions.
  The figures are supplied by the manufacturer from thier own testing.
  It may not be the exact answer you want for the exact pultrusion you are looking for.  There is no other way of getting more figures without individually testing each pultrusion size as well as a number of lengths.                 
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |