Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
waste and kevlar use
waste and kevlar use
Post Reply
Like
3
waste and kevlar use
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
brasco
brasco
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 192,
Visits: 305
how do you use your cloth waste? the unused odds and ends?
and does anyone here use kevlar?
CarbonFiberCreations
Reply
Like
3
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
I infuse my off cuts on a piece of glass. Once cured I cut them into 5cm x 5cm squares and send/show customers if they ask for samples.
I use Kevlar as backing layers on parts prone to impact such as Body Panels for race cars.
Carbon
Copies Ltd
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search