how do you use your cloth waste? the unused odds and ends?
and does anyone here use kevlar?
By wozza
-
2/16/2013 8:03:18 PM
I infuse my off cuts on a piece of glass. Once cured I cut them into 5cm x 5cm squares and send/show customers if they ask for samples.
I use Kevlar as backing layers on parts prone to impact such as Body Panels for race cars.