Pleased ish. I must have got some specs of dust when I applied the release agent too the mould ahhhhhhhhh. You can see the white flecks against the black in places.

Carbon Copies Ltd
Edited 12 Years Ago by wozza
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Thats a nice finish!  You must be pleased with that?
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Finished the Belly Pan. The customer asked for a Black gloss finish so I used 4 layers of Carbon/Kevlar and a black gelcoat.

Warren

Carbon Copies Ltd
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
No worries. As Fred say's if I can help answer any questions please just ask. Don't want you loosing momentumSmile

Warren

Carbon Copies Ltd
Jack.Strong
Jack.Strong
Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)
Group: Forum Members
Posts: 52, Visits: 549
Sorry for the hijack Warren Tongue
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi Fred, is the question for me or Jack?

Warren

Carbon Copies Ltd
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
What do you need to know?

Fred
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Not my bike I'm afraid. It's for a customers Hayabusa. The belly pan will double up as an oil catch tank.

Warren

Carbon Copies Ltd
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
What bike you running?  A friend of mine used to run a twin fueller.
Jack.Strong
Jack.Strong
Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)
Group: Forum Members
Posts: 52, Visits: 549
Apart from CFD, not much Tongue Never get answers to my questions which kind of slows the development and commitment