After 3 days of shaping foam, sanding body filler, spraying 3 coats of high build primer and 3 coats of clear I finally have something I can take a mould from.Smile

Warren
By wozza - 2/14/2013 9:31:58 AM

Pleased ish. I must have got some specs of dust when I applied the release agent too the mould ahhhhhhhhh. You can see the white flecks against the black in places.